Alloy | Density approx. | Composition in % | Important tempers | Tensile Strength Rm N/mm2 | Yield Stress Rp0,2 N/mm2 | Elongation A % |
Hardness HB | Electr. conductivity MS/s | |
---|---|---|---|---|---|---|---|---|---|
Cu-ETP DIN EN 13601 | CW004A | 8,9 | Cu ≥ 99,90 incl. Ag ≤ 0,015 O ≤ 0,040 |
Bars M R300 R250 | ≥ 300 ≥ 250 | ≥ 260 ≥ 180 | ≥ 8 ≥ 15 | HB 75 - 100 HB 65 - 90 | ≥ 57,0 ≥ 57,0 |
Comparable Specifications: |
![](/fileadmin/_processed_/8/e/csm_example_1_aabdb55d2d.jpg)
![](/fileadmin/_processed_/a/e/csm_example_2_7151fee38c.jpg)
![](/fileadmin/_processed_/4/9/csm_example_3_fdd3c1da4b.jpg)